Böhler Welding, TIG rod, creep-resistant CrMo steels

BÖHLER DMO TIG rod

EN ISO classificationO IV
AWS classificationR60-G
Price on request
Give us the diameter and the quantity, we will quote during working hours

Spawlab is the data controller. We will use your data only for replying to this price enquiry. See the privacy policy for details.

Authorised distributorvoestalpine Böhler Welding
Courier shippingfrom the warehouse in Krotoszyn
Data sheetcomposition, properties, specifications
Wire selectionhelp from a welding engineer
Manufacturer data sheet
Application

What BÖHLER DMO TIG rod is used for

BÖHLER DMO is a TIG rod for welding creep-resistant CrMo steels. It is used on boilers, steam pipelines, refinery installations and parts working at elevated temperature.

The rod joins grades such as S235JR, S275JR, S275N, S275M, P195GH, P295GH and P195TR1, along with related materials. The copper coated surface improves current pick-up in the contact tip and smooth feeding, and the rod works in power plant on superheaters, headers and pressure pipework.

  • Classification EN ISO: O IV
  • AWS classification: R60-G
  • Diameters: 1.6 / 2.0 / 2.4 / 3.0 mm

Watch the hydrogen level, dry consumables and a preheated groove are your basic protection against cold cracking. Keep the rod inside the gas shield even after you lift it from the pool, a cold oxidised end will contaminate the next drop. Set the gas post-flow long enough for the pool and the electrode to cool under the shield. Thinner diameters suit root runs and thin sheet, thicker ones suit filling.

Manufacturer datasheet

Chemical composition and properties from the manufacturer datasheet

Datasheet PDF

Typical weld metal values from the voestalpine Böhler Welding data sheet, issue 10/2025. The minimum or the range guaranteed by the maker is given in brackets. The figures depend on the heat treatment condition and the shielding gas stated in the row and do not replace testing the joint to your own WPS.

Chemical composition, wt.-%
CSiMnMo
0,10,61,10,5
Welding data and approvals
Polaritydirect current, electrode negative (DC-)
Shielding gas to EN ISO 14175I1
ApprovalsTÜV (00020, 08066), DB (42.132.72), BV, DNV, CE
Datasheet edition10/2025
Mechanical properties of the all-weld metal, typical values
Condition Yield strength Re, MPa Tensile strength Rm, MPa Elongation A, % Impact energy KV, J at 20 °C Impact energy KV, J at -30 °C
a 530 (min. 470) 650 (range 550 to 740) 26 (min. 22) 180 (min. 130) 100 (min. 80)
s 480 (min. 470) 585 (min. 550) 27 (min. 22) 210 (min. 150) 180 (min. 130)
  • a: as welded
  • s: stress relieved (620 °C / 1 h)
Fits

For which materials and machines

Base materials
  • S235JR
  • S275JR
  • S275N
  • S275M
  • P195GH
  • P295GH
  • P195TR1
  • P265TR1
  • P195TR2
  • P265TR2
  • ASTM A 29
Process and machines

TIG rod, works on any sound machine for this process: welders.

Used welders New welders Ask us to help you choose
Technical substitute

A substitute for this consumable

We will find a substitute with the same classification, diameter and shielding gas over the phone: +48 669 162 833.

From the same group

Other consumables for the same material

For comparison before you buy. A technical substitute is listed above.

All: TIG welding rods