Böhler Welding, TIG rod, stainless and acid-resistant steels

BÖHLER Q T 309L TIG rod

EN ISO classification14343-A W 23 12 L
AWS classificationA5.9 / SFA-5.9 ER309L
Shielding gasI1: 100 % argon
ApprovalsTÜV (19795), DB (43.132.92), CE
from62.77 EURnet
from77.21 EURgross

We ship within 2 working days.

International shipping: calculate the cost

Price for 1 unit, based on the carrier's price list. In the cart we calculate the exact cost for the whole order.

Diameters 1,6 mm are priced on request, tell us the quantity

Spawlab is the data controller. We will use your data only for replying to this price enquiry. See the privacy policy for details.

Authorised distributorvoestalpine Böhler Welding
Courier shippingfrom the warehouse in Krotoszyn
Data sheetcomposition, properties, specifications
Wire selectionhelp from a welding engineer
Manufacturer data sheet
Application

What BÖHLER Q T 309L TIG rod is used for

BÖHLER Q T 309L is a high alloyed austenitic stainless TIG rod. Typical work covers tanks, process installations, food and chemical industry equipment and structures in contact with water and steam.

The rod suits grades such as P295GH and P355N. Its deposit has an austenitic structure that resists corrosion.

  • Classification EN ISO: 14343-A W 23 12 L
  • AWS classification: A5.9 / SFA-5.9 ER309L
  • Shielding gas: I1
  • Diameters: 1.6 / 2.0 / 2.4 / 3.2 mm
  • Approvals: TÜV (19795), DB (43.132.92), CE

Keep the heat input down and do not hold the joint hot longer than you need to, austenite expands strongly and pulls the structure out of shape. Protect the root when you weld from one side, an oxidised underside spoils the corrosion resistance. Keep the rod inside the gas shield even after you lift it from the pool, a cold oxidised end will contaminate the next drop.

Manufacturer datasheet

Chemical composition and properties from the manufacturer datasheet

Datasheet PDF

Typical weld metal values from the voestalpine Böhler Welding data sheet, issue 01/2022. The minimum or the range guaranteed by the maker is given in brackets. The figures depend on the heat treatment condition and the shielding gas stated in the row and do not replace testing the joint to your own WPS.

Chemical composition, wt.-%
CSiMnCrNi
0,020,51,723,513,2
Welding data and approvals
Polaritydirect current, electrode negative (DC-)
Shielding gas to EN ISO 14175I1
ApprovalsTÜV (19795), DB (43.132.92), CE
Datasheet edition01/2022
Mechanical properties of the all-weld metal, typical values
Condition Yield strength Re, MPa Tensile strength Rm, MPa Elongation A, % Impact energy KV, J at 20 °C
u 440 (min. 320) 580 (min. 520) 34 (min. 25) 150 (min. 47)
  • u: untreated, as-welded, shielding gas Ar
Fits

For which materials and machines

Base materials
  • P295GH
  • P355N
Process and machines

TIG rod, works on any sound machine for this process: welders. Shielding gas: I1: 100 % argon.

Used welders New welders Ask us to help you choose
Technical substitute

Consumables with the same classification

Same material group, matching classification, a shared diameter and the same shielding gas. Confirm any substitute for your WPS in the documentation.

From the same group

Other consumables for the same material

For comparison before you buy. A technical substitute is listed above.

All: TIG welding rods
from62.77 EURnet
from77.21 EURgross
Choose a variant