Thermanit, TIG rod, stainless and acid-resistant steels

Thermanit 309 H TIG rod

EN ISO classification14343-A W 22 12 H
AWS classificationA5.9 / SFA-5.9 ER309 (mod.)
Shielding gasI1: 100 % argon
Price on request
Give us the diameter and the quantity, we will quote during working hours

Spawlab is the data controller. We will use your data only for replying to this price enquiry. See the privacy policy for details.

Authorised distributorvoestalpine Böhler Welding
Courier shippingfrom the warehouse in Krotoszyn
Data sheetcomposition, properties, specifications
Wire selectionhelp from a welding engineer
Manufacturer data sheet
Application

What Thermanit 309 H TIG rod is used for

Thermanit 309 H is a high alloyed austenitic stainless TIG rod. It works on pressure vessels, pipework and austenitic steel structures where corrosion resistance matters.

Base materials include 1.4826, 1.4828, 1.4833, X12CrNi23-13, 1.4710, 1.4713 and 1.4724. The rod is used on boilers and pressure vessels under statutory inspection, and its deposit has an austenitic structure that resists corrosion.

  • Classification EN ISO: 14343-A W 22 12 H
  • AWS classification: A5.9 / SFA-5.9 ER309 (mod.)
  • Shielding gas: I1
  • Diameters: 1.6 / 2.0 / 2.4 mm

Keep the heat input down and do not hold the joint hot longer than you need to, austenite expands strongly and pulls the structure out of shape. Grind the tungsten tip along its axis and hold a short arc, otherwise the pool spreads. Protect the root when you weld from one side, an oxidised underside spoils the corrosion resistance. Thinner diameters suit root runs and thin sheet, thicker ones suit filling.

Manufacturer datasheet

Chemical composition and properties from the manufacturer datasheet

Datasheet PDF

Typical weld metal values from the voestalpine Böhler Welding data sheet, issue 01/2024. The minimum or the range guaranteed by the maker is given in brackets. The figures depend on the heat treatment condition and the shielding gas stated in the row and do not replace testing the joint to your own WPS.

Chemical composition, wt.-%
CSiMnCrNi
0,11,11,622,511,5
Welding data and approvals
Polaritydirect current, electrode negative (DC-)
Shielding gas to EN ISO 14175I1
Datasheet edition01/2024
Mechanical properties of the all-weld metal, typical values
Condition Yield strength Re, MPa Tensile strength Rm, MPa Elongation A, % Impact energy KV, J at 20 °C
u 500 (min. 350) 630 (min. 550) 32 (min. 25) 115 (min. 65)
  • u: untreated, as-welded, shielding gas Ar
Fits

For which materials and machines

Base materials
  • 1.4826
  • 1.4828
  • 1.4833
  • X12CrNi23-13
  • 1.4710
  • 1.4713
  • 1.4724
  • 1.4740
  • 1.4742
  • AISI 305
  • ASTM A 297
Process and machines

TIG rod, works on any sound machine for this process: welders. Shielding gas: I1: 100 % argon.

Used welders New welders Ask us to help you choose
Technical substitute

A substitute for this consumable

We will find a substitute with the same classification, diameter and shielding gas over the phone: +48 669 162 833.

From the same group

Other consumables for the same material

For comparison before you buy. A technical substitute is listed above.

All: TIG welding rods