UTP Maintenance, stick electrode, nickel alloys

UTP 80 M stick electrode

EN ISO classificationEN ISO 14172: E Ni 4060 (NiCu30Mn3Ti)
AWS classificationAWS A5.11 / SFA-5.11: ENiCu-7
ApprovalsTÜV (No. 00248), ABS, DNV
Price on request
Give us the diameter and the quantity, we will quote during working hours

Spawlab is the data controller. We will use your data only for replying to this price enquiry. See the privacy policy for details.

Authorised distributorvoestalpine Böhler Welding
Courier shippingfrom the warehouse in Krotoszyn
Data sheetcomposition, properties, specifications
Wire selectionhelp from a welding engineer
Manufacturer data sheet
Application

What UTP 80 M stick electrode is used for

UTP 80 M is a basic coated nickel base electrode of the E Ni 4060 / ENiCu-7 type. The manufacturer intended it for welding and surfacing nickel copper alloys and steels clad with them, above all the grades 2.4360 (NiCu30Fe) and 2.4375 (NiCu30Al). The electrode also suits dissimilar joints: steel to copper and copper alloys, and steel to nickel copper alloys.

Materials of this kind work in apparatus for the chemical and petrochemical industries, and a separate field is seawater evaporation plants and marine equipment, because the deposit takes contact with seawater. The arc is soft and stable, the slag comes off easily and the weld surface comes out smooth. Welding is done in all positions except vertical-down.

  • Classification EN ISO 14172: E Ni 4060 (NiCu30Mn3Ti)
  • AWS classification A5.11 / SFA-5.11: ENiCu-7
  • Coating: basic
  • Current: DC+
  • Diameters: 2.5 / 3.2 / 4.0 mm
  • Lengths: 300 and 350 mm
  • Approvals: TÜV (nr 00248), ABS, DNV

A nickel copper alloy carries the heat away faster than stainless steel, so on heavier sections preheat the part rather than raising the current. The pool is thick, so guide the electrode slowly and see to it that the groove faces have time to fuse. On clad plate weld the steel layer first and add the cladding at the end, after cleaning the transition. Smooth the surfaces that work in seawater, because crevice corrosion starts in notches.

Manufacturer datasheet

Chemical composition and properties from the manufacturer datasheet

Datasheet PDF

Typical weld metal values from the voestalpine Böhler Welding data sheet, issue 09/2025. The minimum or the range guaranteed by the maker is given in brackets. The figures depend on the heat treatment condition and the shielding gas stated in the row and do not replace testing the joint to your own WPS.

Welding data and approvals
Polaritydirect current, electrode positive (DC+)
ApprovalsTÜV (No. 00248), ABS, DNV
Datasheet edition09/2025
Fits

For which materials and machines

Base materials

Material group: nickel alloys. The exact grades and thicknesses are in the manufacturer data sheet, and for an unusual joint call us, we will pick the filler metal.

current: DC+

Process and machines

Stick electrode, works on any sound machine for this process: welders.

Used welders New welders Ask us to help you choose
Technical substitute

A substitute for this consumable

We will find a substitute with the same classification, diameter and shielding gas over the phone: +48 669 162 833.

From the same group

Other consumables for the same material

For comparison before you buy. A technical substitute is listed above.