UTP Maintenance, TIG rod, nickel alloys

UTP A 6170 Co TIG rod

EN ISO classification18274 S Ni 6617 (NiCr22Co12Mo9)
AWS classificationA5.14 / SFA-5.14 ERNiCrCoMo-1
ApprovalsTÜV (05450)
from960.49 EURnet
from1,181.40 EURgross

We ship within 2 working days.

International shipping: calculate the cost

Price for 1 unit, based on the carrier's price list. In the cart we calculate the exact cost for the whole order.

Diameters 2,0 mm, 3,2 mm are priced on request, tell us the quantity

Spawlab is the data controller. We will use your data only for replying to this price enquiry. See the privacy policy for details.

Authorised distributorvoestalpine Böhler Welding
Courier shippingfrom the warehouse in Krotoszyn
Data sheetcomposition, properties, specifications
Wire selectionhelp from a welding engineer
Manufacturer data sheet
Application

What UTP A 6170 Co TIG rod is used for

UTP A 6170 Co is a TIG rod in a NiCrCo alloy for high temperature applications up to 1100 degrees C. It works on boiler components, furnace parts, chemical installations and heat exchangers exposed to aggressive media.

Base materials are 1.4958, UNS N08810, 1.4959, UNS N08811, NiCr23Co12Mo and UNS N06617. You feed the filler into the pool by hand while the arc burns between the tungsten electrode and the weld.

  • Classification EN ISO: 18274 S Ni 6617 (NiCr22Co12Mo9)
  • AWS classification: A5.14 / SFA-5.14 ERNiCrCoMo-1
  • Diameters: 1.6 / 2.0 / 2.4 / 3.2 mm
  • Approvals: TÜV (05450)

Move the pool more slowly than on steel, nickel alloys are sluggish and will not flow to the groove edges on their own. Keep the rod inside the gas shield even after you lift it from the pool, a cold oxidised end will contaminate the next drop. Set the gas post-flow long enough for the pool and the electrode to cool under the shield. Match the diameter to the material thickness and the welding position, thinner rods are easier to control out of position.

Manufacturer datasheet

Chemical composition and properties from the manufacturer datasheet

Datasheet PDF

Typical weld metal values from the voestalpine Böhler Welding data sheet, issue 05/2023. The minimum or the range guaranteed by the maker is given in brackets. The figures depend on the heat treatment condition and the shielding gas stated in the row and do not replace testing the joint to your own WPS.

Chemical composition, wt.-%
CSiCrNiMoCoTiFeAl
0,060,122,0balance8,511,50,41,01,0
Welding data and approvals
Polaritydirect current, electrode negative (DC-)
Shielding gas to EN ISO 14175I1,R1
ApprovalsTÜV (05450)
Datasheet edition05/2023
Mechanical properties of the all-weld metal, typical values
Condition Yield strength Re, MPa Tensile strength Rm, MPa Elongation A, % Impact energy KV, J at 20 °C
u 450 750 30 120
  • u: untreated, as-welded
Fits

For which materials and machines

Base materials
  • 1.4958
  • UNS N08810
  • 1.4959
  • UNS N08811
  • NiCr23Co12Mo
  • UNS N06617
Process and machines

TIG rod, works on any sound machine for this process: welders.

Used welders New welders Ask us to help you choose
Technical substitute

A substitute for this consumable

We will find a substitute with the same classification, diameter and shielding gas over the phone: +48 669 162 833.

From the same group

Other consumables for the same material

For comparison before you buy. A technical substitute is listed above.

All: Hardfacing and reclamation consumables
from960.49 EURnet
from1,181.40 EURgross
Choose a variant