Thermanit, solid MIG/MAG wire, stainless and acid-resistant steels

Thermanit X solid MIG/MAG wire

EN ISO classification14343-A G 18 8 Mn
AWS classificationA5.9 / SFA-5.9 ER307(mod.)
Shielding gasM12: Ar with CO2 added (up to 5 %), M13: Ar with O2 added (up to 3 %), M21: Ar with 15 to 25 % CO2
ApprovalsTÜV (05651), DB (43.132.01), DNV, VG 95132-1, CE
from243.72 EURnet
from299.77 EURgross

We ship within 2 working days.

International shipping: calculate the cost

Price for 1 unit, based on the carrier's price list. In the cart we calculate the exact cost for the whole order.

Diameters 0,8 mm, 1,6 mm are priced on request, tell us the quantity

Spawlab is the data controller. We will use your data only for replying to this price enquiry. See the privacy policy for details.

Authorised distributorvoestalpine Böhler Welding
Courier shippingfrom the warehouse in Krotoszyn
Data sheetcomposition, properties, specifications
Wire selectionhelp from a welding engineer
Manufacturer data sheet
Application

What Thermanit X solid MIG/MAG wire is used for

Thermanit X is a high-alloyed solid wire for special applications. It suits welding stainless and acid-resistant steels in tank building, process piping and equipment for the chemical and food industries.

The wire suits hand work with a semiautomatic torch and mechanised stations, and it also serves for cladding carbon steel surfaces.

  • Classification EN ISO: 14343-A G 18 8 Mn
  • AWS classification: A5.9 / SFA-5.9 ER307(mod.)
  • Shielding gas: M12, M13, M21
  • Diameters: 0.8 / 0.9 / 1.0 / 1.2 / 1.6 mm
  • Approvals: TÜV (05651), DB (43.132.01), DNV, VG 95132-1, CE

Keep the heat input down and do not hold the joint hot longer than needed, austenite expands strongly and pulls the structure out of shape. Check the contact tip, a worn bore upsets the wire feed and causes burnback. Match the drive rolls to the wire diameter and check the liner, wire slip shows up at once in an unstable arc. Match the diameter to the thickness and the position, thinner wires are easier to control in constrained positions.

Manufacturer datasheet

Chemical composition and properties from the manufacturer datasheet

Datasheet PDF

Typical weld metal values from the voestalpine Böhler Welding data sheet, issue 05/2023. The minimum or the range guaranteed by the maker is given in brackets. The figures depend on the heat treatment condition and the shielding gas stated in the row and do not replace testing the joint to your own WPS.

Chemical composition, wt.-%
CSiMnCrNi
0,080,87,0199,0
Welding data and approvals
Polaritydirect current, electrode positive (DC+)
Shielding gas to EN ISO 14175M1
ApprovalsTÜV (05651), DB (43.132.01), DNV, VG 95132-1, CE
Datasheet edition05/2023
Mechanical properties of the all-weld metal, typical values
Condition Yield strength Re, MPa Tensile strength Rm, MPa Elongation A, % Impact energy KV, J at -60 °C Impact energy KV, J at -110 °C
u 430 (min. 370) 640 (min. 600) 42 (min. 35) 60 (min. 47) 32
  • u: untreated, as-welded, shielding gas Ar + 2.5% CO 2
Fits

For which materials and machines

Base materials

Material group: stainless and acid-resistant steels. The exact grades and thicknesses are in the manufacturer data sheet, and for an unusual joint call us, we will pick the filler metal.

Process and machines

Solid MIG/MAG wire, works on any sound machine for this process: welders. Shielding gas: M12: Ar with CO2 added (up to 5 %), M13: Ar with O2 added (up to 3 %), M21: Ar with 15 to 25 % CO2.

Used welders New welders Ask us to help you choose
Technical substitute

Consumables with the same classification

Same material group, matching classification, a shared diameter and the same shielding gas. Confirm any substitute for your WPS in the documentation.

From the same group

Other consumables for the same material

For comparison before you buy. A technical substitute is listed above.

All: Solid MIG/MAG wires
from243.72 EURnet
from299.77 EURgross
Choose a variant