Böhler Welding, flux-cored wire, stainless and acid-resistant steels

FOXcore 317L-T0 flux-cored wire

EN ISO classification17633-A T Z 19 13 4 N L R M21 (C1) 3
AWS classificationA5.22 / SFA-5.22 E317LT0-4(1)
Shielding gasC1: 100 % CO2, M21: Ar with 15 to 25 % CO2
ApprovalsCE
Price on request
Give us the diameter and the quantity, we will quote during working hours

Spawlab is the data controller. We will use your data only for replying to this price enquiry. See the privacy policy for details.

Authorised distributorvoestalpine Böhler Welding
Courier shippingfrom the warehouse in Krotoszyn
Data sheetcomposition, properties, specifications
Wire selectionhelp from a welding engineer
Manufacturer data sheet
Application

What FOXcore 317L-T0 flux-cored wire is used for

FOXcore 317L-T0 is a high-alloyed austenitic stainless flux-cored wire of the E 317L type for corrosion resistant austenitic steels with a higher Mo content and for claddings on mild steel, meant for the flat and horizontal positions under a mixed shielding gas.

It joins grades such as 1.4429, 1.4434, 1.4435, 1.4438, 1.4439, AISI 316L and 316LN together with their equivalents. The wire goes on offshore structures, where the joint works in a marine environment, and the deposit resists intergranular corrosion.

  • Classification EN ISO: 17633-A T Z 19 13 4 N L R M21 (C1) 3
  • AWS classification: A5.22 / SFA-5.22 E317LT0-4(1)
  • Shielding gas: M21, C1
  • Diameters: 1.2 / 1.5 mm
  • Approvals: CE

After welding remove the heat tint by pickling or brushing, the oxide layer alone lowers the corrosion resistance of the joint. Remove the slag before every following bead, slag left between layers is the most common source of inclusions. Store the wire dry and do not leave an open spool in the feeder overnight, the core takes up moisture.

Manufacturer datasheet

Chemical composition and properties from the manufacturer datasheet

Datasheet PDF

Typical weld metal values from the voestalpine Böhler Welding data sheet, issue 04/2021. The minimum or the range guaranteed by the maker is given in brackets. The figures depend on the heat treatment condition and the shielding gas stated in the row and do not replace testing the joint to your own WPS.

Welding data and approvals
Polaritydirect current, electrode positive (DC+)
Shielding gas to EN ISO 14175M2
ApprovalsCECE
Datasheet edition04/2021
Mechanical properties of the all-weld metal, typical values
Condition Yield strength Re, MPa Tensile strength Rm, MPa Elongation A, % Impact energy KV, J at 20 °C Impact energy KV, J at -60 °C
u 420 (min. 350) 570 (min. 550) 32 (min. 25) 50 45 (min. 32)
  • u: untreated, as-welded, shielding gas M21 (Ar + 18% CO2)
Fits

For which materials and machines

Base materials
  • 1.4429
  • 1.4434
  • 1.4435
  • 1.4438
  • 1.4439
  • AISI 316L
  • 316LN
  • 317L
  • 317LN
  • UNS S31600
Process and machines

Flux-cored wire, works on any sound machine for this process: welders. Shielding gas: C1: 100 % CO2, M21: Ar with 15 to 25 % CO2.

Used welders New welders Ask us to help you choose
Technical substitute

A substitute for this consumable

We will find a substitute with the same classification, diameter and shielding gas over the phone: +48 669 162 833.

From the same group

Other consumables for the same material

For comparison before you buy. A technical substitute is listed above.