Thermanit, solid MIG/MAG wire, stainless and acid-resistant steels

Thermanit GE-316L Si solid MIG/MAG wire

EN ISO classification14343-A G 19 12 3 L Si
AWS classificationA5.9 / SFA-5.9 ER316LSi
Shielding gasM12: Ar with CO2 added (up to 5 %), M13: Ar with O2 added (up to 3 %)
ApprovalsTÜV (00489), DB (43.132.10), DNV, ABS, BV, LR (spec. List), CE
Price on request
Give us the diameter and the quantity, we will quote during working hours

Spawlab is the data controller. We will use your data only for replying to this price enquiry. See the privacy policy for details.

Authorised distributorvoestalpine Böhler Welding
Courier shippingfrom the warehouse in Krotoszyn
Data sheetcomposition, properties, specifications
Wire selectionhelp from a welding engineer
Manufacturer data sheet
Application

What Thermanit GE-316L Si solid MIG/MAG wire is used for

Thermanit GE-316L Si is a high-alloyed austenitic stainless solid wire. It works on pressure vessels, process piping and austenitic structures where corrosion resistance counts.

Among the parent materials it covers 1.4401, 1.4404, 1.4409, 1.4429, 1.4432, 1.4435 and 1.4436. The wire also suits cladding runs on steel, and the deposit has an austenitic structure.

  • Classification EN ISO: 14343-A G 19 12 3 L Si
  • AWS classification: A5.9 / SFA-5.9 ER316LSi
  • Shielding gas: M12, M13
  • Diameters: 0.8 / 0.9 / 1.0 / 1.2 / 1.6 / 2.0 mm
  • Approvals: TÜV (00489), DB (43.132.10), DNV, ABS, BV, LR (spec. List), CE

Keep the heat input down and do not hold the joint hot longer than needed, austenite expands strongly and pulls the structure out of shape. Check the contact tip, a worn bore upsets the wire feed and causes burnback.

Manufacturer datasheet

Chemical composition and properties from the manufacturer datasheet

Datasheet PDF

Typical weld metal values from the voestalpine Böhler Welding data sheet, issue 02/2025. The minimum or the range guaranteed by the maker is given in brackets. The figures depend on the heat treatment condition and the shielding gas stated in the row and do not replace testing the joint to your own WPS.

Chemical composition, wt.-%
CSiMnCrNiMo
0,020,81,718,412,42,8
Welding data and approvals
Polaritydirect current, electrode positive (DC+)
Shielding gas to EN ISO 14175M11, M12, M13
Heat inputmax. 2,0 kJ/mm
Interpass temperaturemax. 150 °C
Maximum service temperature400 °C
Service at low temperaturesdown to -196 °C
Heat treatment after weldingusually not needed; if required, solution annealing at 1050 °C and cooling in water
Shielding gas per data sheetAr + 2 % CO2, Ar + 2 to 3 % CO2 or Ar + 0 to 5 % H2 + 0 to 5 % CO2
ApprovalsTÜV (00489), DB (43.132.10), DNV, ABS, BV, LR, CE
Datasheet edition02/2025
Mechanical properties of the all-weld metal, typical values
Condition Yield strength Re, MPa Tensile strength Rm, MPa Elongation A, % Impact energy KV, J at 20 °C Impact energy KV, J at -196 °C
u 430 (min. 320) 580 (min. 510) 38 (min. 25) 120 (min. 75) 45 (min. 32)
  • u: Untreated, as-welded, shielding gas Ar + 2.5% CO 2
Fits

For which materials and machines

Base materials
  • 1.4401
  • 1.4404
  • 1.4409
  • 1.4429
  • 1.4432
  • 1.4435
  • 1.4436
  • 1.4571
  • 1.4580
  • 1.4583
  • UNS S31600
  • AISI 316L
Process and machines

Solid MIG/MAG wire, works on any sound machine for this process: welders. Shielding gas: M12: Ar with CO2 added (up to 5 %), M13: Ar with O2 added (up to 3 %).

Used welders New welders Ask us to help you choose
Technical substitute

Consumables with the same classification

Same material group, matching classification, a shared diameter and the same shielding gas. Confirm any substitute for your WPS in the documentation.

From the same group

Other consumables for the same material

For comparison before you buy. A technical substitute is listed above.

All: Solid MIG/MAG wires