Böhler Welding, flux-cored wire, stainless and acid-resistant steels

FOXcore 13/4-MC F metal-cored wire

EN ISO classification17633-A T 13 4 M M12 2
AWS classificationA5.22 / SFA-5.22 EC410NiMo (mod.)
Shielding gasM12: Ar with CO2 added (up to 5 %)
ApprovalsCE
Price on request
Give us the diameter and the quantity, we will quote during working hours

Spawlab is the data controller. We will use your data only for replying to this price enquiry. See the privacy policy for details.

Authorised distributorvoestalpine Böhler Welding
Courier shippingfrom the warehouse in Krotoszyn
Data sheetcomposition, properties, specifications
Wire selectionhelp from a welding engineer
Manufacturer data sheet
Application

What FOXcore 13/4-MC F metal-cored wire is used for

FOXcore 13/4-MC F is a high alloyed, soft martensitic stainless metal-cored wire of the E410NiMo type, made for foundry applications. It is used on process installations, heat exchangers, sanitary structures and parts exposed to corrosion.

The wire suits grades such as 1.4313, 1.4317, 1.4407, 1.4414 and UNS S41500. Its high deposition rate shortens the time needed to fill heavier grooves, and the deposit has a martensitic structure with a lowered carbon content.

  • Classification EN ISO: 17633-A T 13 4 M M12 2
  • AWS classification: A5.22 / SFA-5.22 EC410NiMo (mod.)
  • Shielding gas: M12
  • Diameters: 1.2 / 1.5 / 1.6 mm
  • Approvals: CE

Keep the interpass temperature low and the beads narrow, overheating promotes carbide precipitation and distortion. Keep the gas cover complete, without a full slag layer the pool is more sensitive to draughts. Check the feed roll pressure, a metal-cored wire is easier to crush than a solid one. Match the diameter to the material thickness and the welding position, thinner wires are easier to control out of position.

Manufacturer datasheet

Chemical composition and properties from the manufacturer datasheet

Datasheet PDF

Typical weld metal values from the voestalpine Böhler Welding data sheet, issue 04/2021. The minimum or the range guaranteed by the maker is given in brackets. The figures depend on the heat treatment condition and the shielding gas stated in the row and do not replace testing the joint to your own WPS.

Chemical composition, wt.-%
CSiMnCrNiMo
0,0230,70,912,24,60,6
Welding data and approvals
Polaritydirect current, electrode positive (DC+)
Shielding gas to EN ISO 14175M12
ApprovalsCE
Datasheet edition04/2021
Mechanical properties of the all-weld metal, typical values
Condition Yield strength Re, MPa Tensile strength Rm, MPa Elongation A, % Impact energy KV, J at 20 °C Impact energy KV, J at -20 °C
a 745 (min. 500) 900 (min. 760) 16 (min. 15) 55 (min. 50) 50 (min. 47)
a1 700 840 18 - 50
  • a: annealed/tempered, 600°C for 2 h / furnace cooling to 300°C followed by air cooling, shielding gas M12 (Ar + 2.5% CO2)
  • a1: annealed/tempered, 580°C for 12 h / furnace cooling to 300°C followed by air cooling, shielding gas M12 (Ar + 2.5% CO2)
Fits

For which materials and machines

Base materials
  • 1.4313
  • 1.4317
  • 1.4407
  • 1.4414
  • UNS S41500
Process and machines

Flux-cored wire, works on any sound machine for this process: welders. Shielding gas: M12: Ar with CO2 added (up to 5 %).

Used welders New welders Ask us to help you choose
Technical substitute

Consumables with the same classification

Same material group, matching classification, a shared diameter and the same shielding gas. Confirm any substitute for your WPS in the documentation.

From the same group

Other consumables for the same material

For comparison before you buy. A technical substitute is listed above.

All: Flux-cored wires